Dikici, B.Tekmen, C.Gavgali, M.Tsunekawa, Y.2025-05-102025-05-10200797849311360522-s2.0-85076871279https://hdl.handle.net/20.500.14720/18120The corrosion behaviors of T8 tempered Al-Si-Mg/SiCp metal matrix composites (MMCs) were investigated in aerated and deaerated 3.5wt% NaCl solutions by potentiodynamic polarization technique in this study. In order to determine the effect of cold work on the electrochemical behavior, the composites were cold-worked to a plastic strain of 4, 6, 10, 25 and 50%. A major change in the corrosion morphologies were observed cold working ratio increased from 4 to 50%. For example, electrochemical analysis indicated that the corrosion current densities (icor) of 20% vol. SiC composite increased from 0.8 to 5.9 with increasing cold-worked ratio after T8 temper. In addition, we find that there is a significant coloration between corrosion susceptibility and level of cold work.eninfo:eu-repo/semantics/closedAccessCold WorkingCorrosionMetal Matrix CompositeSic ParticleT8 TemperThe Effect of Cold-Worked Ratio on Corrosion Behavior of T8 Tempered Al-si-mg/Sicp Metal Matrix CompositesConference ObjectN/AN/A