A Comparative Study: the Combined Effect of the Cold Working and Age Hardening Processes on Pitting Behaviour of Al/Sic Metal Matrix Composites Under Saline Environment
dc.authorid | Dikici, Burak/0000-0002-7249-923X | |
dc.authorid | Tekmen, Cagri/0000-0002-6742-6247 | |
dc.authorscopusid | 23501298200 | |
dc.authorscopusid | 6602459745 | |
dc.authorwosid | Tekmen, Cagri/Mfk-0164-2025 | |
dc.authorwosid | Dikici, Burak/A-2054-2009 | |
dc.contributor.author | Dikici, Burak | |
dc.contributor.author | Tekmen, Cagri | |
dc.date.accessioned | 2025-05-10T17:39:44Z | |
dc.date.available | 2025-05-10T17:39:44Z | |
dc.date.issued | 2016 | |
dc.department | T.C. Van Yüzüncü Yıl Üniversitesi | en_US |
dc.department-temp | [Dikici, Burak] Yuzuncu Yil Univ, Dept Mech Engn, TR-65080 Van, Turkey; [Tekmen, Cagri] Dokuz Eylul Univ, Met & Mat Engn, Izmir, Turkey | en_US |
dc.description | Dikici, Burak/0000-0002-7249-923X; Tekmen, Cagri/0000-0002-6742-6247 | en_US |
dc.description.abstract | The combined effect of cold working and age hardening treatment (T8) on the corrosion behaviour of Al-Si-Mg based metal matrix composite reinforced with silicon carbide particles has been investigated in 3.5wt% NaCl solution by potentiodynamic polarization technique. Composites containing 10 and 20 vol% silicon carbide particles were produced by compocasting technique and cold-worked at ratios of 4, 6, 10, 25 and 50% prior to ageing heat treatment conducted at 175 degrees C Corroded surfaces of the composites were observed by using scanning electron microscopy. A significant change in the corrosion behaviour of composites was observed when cold work ratio was increased from 4 to 50%. In addition, it has been found that the influence of cold working on corrosion behaviour is relatively higher compared to the effect of reinforcement content and age-hardening treatment. | en_US |
dc.description.woscitationindex | Science Citation Index Expanded | |
dc.identifier.doi | 10.1177/0021998315576554 | |
dc.identifier.endpage | 480 | en_US |
dc.identifier.issn | 0021-9983 | |
dc.identifier.issn | 1530-793X | |
dc.identifier.issue | 4 | en_US |
dc.identifier.scopus | 2-s2.0-84955149944 | |
dc.identifier.scopusquality | Q2 | |
dc.identifier.startpage | 471 | en_US |
dc.identifier.uri | https://doi.org/10.1177/0021998315576554 | |
dc.identifier.uri | https://hdl.handle.net/20.500.14720/14986 | |
dc.identifier.volume | 50 | en_US |
dc.identifier.wos | WOS:000368164200003 | |
dc.identifier.wosquality | Q3 | |
dc.language.iso | en | en_US |
dc.publisher | Sage Publications Ltd | en_US |
dc.relation.publicationcategory | Makale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanı | en_US |
dc.rights | info:eu-repo/semantics/closedAccess | en_US |
dc.subject | Metal-Matrix Composite | en_US |
dc.subject | Corrosion | en_US |
dc.subject | Plastic Deformation | en_US |
dc.subject | Casting | en_US |
dc.title | A Comparative Study: the Combined Effect of the Cold Working and Age Hardening Processes on Pitting Behaviour of Al/Sic Metal Matrix Composites Under Saline Environment | en_US |