Effect of Different Disinfectant Methods on the Initial Microtensile Bond Strength of a Self-Etch Adhesive To Dentin

dc.authorid Deniz Arisu, Hacer/0000-0003-0249-8968
dc.authorid Eliguzeloglu Dalkilic, Evrim/0000-0002-1075-9278
dc.authorscopusid 57117844500
dc.authorscopusid 7801441563
dc.authorscopusid 6507212762
dc.authorscopusid 6505906813
dc.authorscopusid 6506911231
dc.authorwosid Arä±Su, Hacer/Aad-9478-2019
dc.authorwosid Dalkılıç, Evrim/Gpk-1321-2022
dc.contributor.author Dalkilic, Evrim Eliguzeloglu
dc.contributor.author Arisu, Hacer Deniz
dc.contributor.author Kivanc, Bagdagul Helvacioglu
dc.contributor.author Uctasli, Mine Betul
dc.contributor.author Omurlu, Huma
dc.date.accessioned 2025-05-10T16:48:13Z
dc.date.available 2025-05-10T16:48:13Z
dc.date.issued 2012
dc.department T.C. Van Yüzüncü Yıl Üniversitesi en_US
dc.department-temp [Dalkilic, Evrim Eliguzeloglu] Yuzuncu Yil Univ, Dept Restorat Dent, Fac Dent, TR-65080 Van, Turkey; [Arisu, Hacer Deniz; Uctasli, Mine Betul; Omurlu, Huma] Gazi Univ, Dept Restorat Dent, Fac Dent, TR-06500 Ankara, Turkey; [Kivanc, Bagdagul Helvacioglu] Gazi Univ, Dept Endodont, Fac Dent, TR-06500 Ankara, Turkey en_US
dc.description Deniz Arisu, Hacer/0000-0003-0249-8968; Eliguzeloglu Dalkilic, Evrim/0000-0002-1075-9278 en_US
dc.description.abstract The aim of this in vitro study was to evaluate the effect of different disinfection methods on the initial microtensile bond strength of a two-step, self-etch adhesive to dentin. Twenty mandibular molars were sectioned parallel to the occlusal plane to expose the mid-coronal dentin. All of the teeth were divided into four groups (n = 5 per group): (1) in group OZ, the dentin surfaces were exposed to ozone gas from the Ozonytron X delivery system (OzonyTron X-Bioozonix, Munich, Germany), (2) in group ND, the dentin surfaces were irradiated with an Nd:YAG laser (Pulsmaster 600 IQ, American Dental Technologies, U.S.), (3) in group CHX, the dentin surfaces were treated with a 2% chlorhexidine solution, and (4) in the control group, no treatment was applied. In all of the groups, the teeth were restored with Clearfil SE Bond (Kuraray, Tokyo, Japan) and Clearfil Majesty Posterior (Kuraray, Tokyo, Japan), according to the manufacturer's instructions. The teeth were sectioned perpendicular to the bonded surface (surface area of approximately 1 mm(2)). Thus, six to seven specimens were obtained from each tooth, and a total of 34 specimens were analyzed in each group. The specimens were attached to the microtensile test machine (Micro Tensile Tester, T-61010 K, Bisco, U.S.). The data was analyzed using the one-way analysis of variance (ANOVA) and Tukey test (p < 0.05). Fracture modes of each specimen were determined using a stereomicroscope (SZ-PT Olympus, Tokyo, Japan) and a scanning electron microscope (SEM). The lowest bond strength occurred in the OZ group. Significant differences were determined only between group OZ and the other groups (group ND, group CHX, and control group) (p < 0.05). In conclusion, although ozone decreased the microtensile bond strength of the self-etch adhesive system to dentin, the Nd:YAG laser and 2% chlorhexidine did not change the microtensile bond strength so in context of the present study it would appear that the Nd:YAG laser and 2% chlorhexidine may be used as pre-restorative sterilization procedures on the dentin prior to the application of a two-step, self-etch adhesive. en_US
dc.description.woscitationindex Science Citation Index Expanded
dc.identifier.doi 10.1007/s10103-011-0987-x
dc.identifier.endpage 825 en_US
dc.identifier.issn 0268-8921
dc.identifier.issn 1435-604X
dc.identifier.issue 4 en_US
dc.identifier.pmid 21915687
dc.identifier.scopus 2-s2.0-84863620799
dc.identifier.scopusquality Q1
dc.identifier.startpage 819 en_US
dc.identifier.uri https://doi.org/10.1007/s10103-011-0987-x
dc.identifier.uri https://hdl.handle.net/20.500.14720/1489
dc.identifier.volume 27 en_US
dc.identifier.wos WOS:000305274100019
dc.identifier.wosquality Q2
dc.language.iso en en_US
dc.publisher Springer London Ltd en_US
dc.relation.publicationcategory Makale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanı en_US
dc.rights info:eu-repo/semantics/closedAccess en_US
dc.subject Ozone en_US
dc.subject Nd:Yag Laser en_US
dc.subject Microtensile en_US
dc.subject Bond Strength en_US
dc.subject Chlorhexidine en_US
dc.title Effect of Different Disinfectant Methods on the Initial Microtensile Bond Strength of a Self-Etch Adhesive To Dentin en_US
dc.type Article en_US